Process Practice for Production of Steel H11Mn2SiA for Welding Wire by 65 t Consteel EBT EAF-LF-CC Flowsheet at Shiheng Steel

Li Hongyong ,Chai Jianming   

  1. Shiheng Special Steel Works,Jinan lron and Steel Group,Feicheng 271612
  • Received:2006-10-31 Online:2007-05-01 Published:2023-02-04

石横特钢65 t Consteel EBT EAF-LF-CC流程生产焊线钢H11Mn2SiA的工艺实践

李洪勇,柴建铭   

  1. 济南钢铁集团石横特殊钢厂,肥城271612
  • 作者简介:李洪勇(1975-),男,工程师,1998年包头钢铁学院钢铁冶 金专业毕业,从事炼钢工艺研究和新产品开发。

Abstract: With  using  60%  hot  metal  +  quality  scrap  charge,Consteel  EAF  eccentric  bottom  tapping  operation,con- trolling    tapping    end [C]    0.035%~0.050%    and    tapping[P]≤0.012%,LF    refining    by    low    basicity    slag,feeding silicon  wire,  soft  blown  argon  for  15  min  after  LF  refining  and  fully  shielding  auto  control  casting  150  mmx150  mm  bilet  in whole period,  the  average oxygen  content  in steel  H11Mn2SiA(0.06~0.09C,0.82~1.00Si,1.45~1.70Mn)for welding  wire  was  20×10-6,of which  the  Φ5.5  mm  wire  rods  could  be  direct  drawn  to  φ1.0  mm  wire  without  by  heat  treatment and  no-broken  wire   occurred.

摘要: 采用60%铁水+优质废钢,Comteel电弧炉偏心底炉出钢留渣作业,控制出钢终点[C]0.035%~0.050%、出钢[P]≤0.012%;LF用低碱度渣精炼,喂硅钙线,LF精炼后软吹氩15 min;150 mm×150 mm方坯连铸时,采用全保护自动控制浇铸和结晶器、铸坯凝固末端电磁搅拌,使所生产的H11Mn2SiA焊线钢(%:0.06~6.09C、0.82~1.00Si、1.45~1.70Mn)的平均氧含量为20×10-6,Φ5.5 mm盘条不经热处理可直接冷拔至Φ1.0 mm不断丝。

关键词: H11Mn2SiA焊线钢, Consteel EAF, LF氧含量