Practice for Semi-Continuous Rolling Process of Φ160 mm 0Cr17N4Cu4Nb Precipitation-Hardening Stainless Steel Bar

Zhao Dezhong   

  1. Special Steel Works,Benxi Iron and Steel(Group)CoLtd,Benxi117001
  • Received:2006-10-19 Online:2007-05-01 Published:2023-02-04

Φ160 mm 0Cr17Ni4Cu4Nb沉淀硬化不锈钢半连续轧制工艺实践

赵德忠   

  1. 本溪钢铁(集团)公司特殊钢厂,本溪117001
  • 作者简介:赵德忠(1972-),男,工程师,1997年辽宁工学院毕业,从事加工工艺的研究与管理。

Abstract: Φ160 mm 0Cr17Ni4Cu4Nb stainless steel bar products are produced at Special Steel Works,Benxi Steel by 3t ESR ingot-800 primary mill blooming 190 mm×190 mm billet - four stand 650 tandem mill rolling process to replace original  3t  ESR  ingot  -forging  process.Practice  indicated  that  production  effciency,yield  and  surface  quality  of products produced by rolling process were better than that by forging process,the go2(Rpo.2)of中160 mm OCr17Ni4Cu4Nb stainiess  steel rolled bar was  890~955  MPa, σb(Rm) 960~1020  MPa,δ5(A)16%~18%,Ψ(Z)61%~65%,δ - Fe≤ 5%  all to meet the requirement  of standard  CB8732Ⅱ .

Key words: Φ160 mm Bar,0Cr17Ni4Cu4Nb Precipitation -Hardening Stainless Steel,Semi - Continuous Rollin, δ-Ferrite

摘要: 本钢特钢厂采用3 t电渣锭-800初轧机开190 mm×190 mm方坯4架650连轧工艺,生产Φ160 mm 0Cr17Ni4Cu4Nb不锈钢棒材以替代原先3 t电渣锭锻造生产工艺。实践表明,轧制工艺生产效率、成材率和钢材表面质量均优于锻制工艺;轧制工艺所生产的中Φ160 mm 0Cr17Ni4Cu4Nb不锈钢σ0.2(Rp0.2)890~955 MPa.σb(Rm) 960~1020 MPa,δ5(A)16%~18%,Ψ(Z)61%~65%,δ-Fe≤5%均满足GB8732Ⅱ的要求。

关键词: φ160 mm棒材, 0Cr17Ni4Cu4Nb沉淀硬化不锈钢, 半连续轧制, δ-铁素体