[1] |
Sun Jian, Liu Zhanli, Li Jie, Zhang Pengfei, Zheng Jinghui, Xing Liyong.
High Temperture Thermoplastic Behavior of BTW1 Steel Continuous Casting Slab
[J]. Special Steel, 2024, 45(6): 12-16.
|
[2] |
Fu Chengzhe, Zhang Shuai, Wang Shuang, Gao Hong, Wang Fuyue, Zhang Zherui.
Thermodynamic Coupling Analysis of Air Cooling for X70 Pipeline Steel Continuous Casting Slab Based on ABAQUS
[J]. Special Steel, 2024, 45(6): 62-68.
|
[3] |
Chen Yufeng, Zhang Junfen, Xue Qihe, Bai Jun, Yang Shufeng, Li Jingshe.
Effect of Nitrogen Content and Final Rolling Temperature on
Low- temperature Impact Toughness of Titanium
Microalloyed High- strength Steel CGLC700
[J]. Special Steel, 2024, 45(3): 40-18.
|
[4] |
Liu Huidan, Yin Licheng, Zhu Jiqiao, Liu Jing, Cheng Zhaoyang, Dai Huilei.
Effect of Aging Rolling Temperature on the Microstructure,
Texture and Magnetic Properties of Low-temperature
Grain-oriented Silicon Steel
[J]. Special Steel, 2024, 45(3): 80-84.
|
[5] |
Chen De, Zhang Guangjun, Liu Jigang.
Process Optimization and Practice on CC Soft Reduction in GCr15 Bearing Steel Billet
[J]. Special Steel, 2024, 45(2): 50-55.
|
[6] |
Su Yongze, Zhang Xingli, Dai Fangyin, Cui Guibo, Chen Xinyan.
Analysis of Surface Defects of High Strength Welding Wire Steel N2M2T Continuous Casting Billet and Process Improvement
[J]. Special Steel, 2024, 45(2): 61-65.
|
[7] |
Wu Xiangyu, Dong Bingcheng , Wang Zifei, Tian Qianren, Fu Jianxun.
Modification Effect and Mechanism of La-Ce on Inclusions in GCr15 Bearing Steel
[J]. Special Steel, 2024, 45(2): 39-45.
|
[8] |
Yu Haochen, Zhang Benguo, Wu Heng, Zhang Ruizhong.
Research on a Steel Leakage Prediction Model Based on One vs Rest Genetic Algorithm Optimization Decision Tree
[J]. Special Steel, 2024, 45(2): 112-117.
|
[9] |
Jiang Yaqing, Chen Jun, Huang Chenggang, Li Bo, Li Qian, Jiang Yanfeng.
Effect of Tundish Coating on Cleanliness of GCr15 Bearing Steel
[J]. Special Steel, 2024, 45(1): 61-64.
|
[10] |
Li Jingshe, Wang Cun, Chen Yongfeng, Yang Shufeng, Liu Wei, Bai Yun, Huang Chengyong, Sun Ye.
Research and Application Progress of Plasma Heating Technology for Continuous Casting Tundish
[J]. Special Steel, 2024, 45(1): 1-11.
|
[11] |
Huo Zhenquan, Yang Lifeng.
Analysis of Metallurgical Quality of Forged Steel Cold Rolling Work Roll and Improvement of ESR Process
[J]. Special Steel, 2023, 44(6): 12-18.
|
[12] |
Liu Chunwei, Zhang Hao, Cao Lei, Wang Guocheng.
Effect of VD Low Basicity Slag on Inclusions of GCr15 Bearing Steel
[J]. Special Steel, 2023, 44(6): 78-82.
|
[13] |
Xue Rundong, Zhao Zhiyi, Fei Aigeng.
Effect of Cold Processing on the Substructure of CN-1515 Austenitic Stainless Steel Cladding Tube
[J]. Special Steel, 2023, 44(5): 107-112.
|
[14] |
Chen Qiwei, Bao Hansheng, Yang Gang, Wang Jingzhong, Chen Genbao, Dai Weixing.
Comparison of High-temperature Processing Properties of Continuous Casting and Die Casting Tube Billets of S30432 Steel
[J]. Special Steel, 2023, 44(5): 97-106.
|
[15] |
Yin Qing, Cao Wenquan, Wu Xiaolin, Wang Cunyu, Wang Hui, Yu Feng.
Research on Rolling Contact Fatigue Mechanism of High Clean Bearing Steel GCr15