Process Practice for Production of Caterpillar Track Steel 35MnBM by 90    t    EAF-LF(VD)-CC-CR    Flow    Sheet

Zhu Zhixin,Li Ai and Wang Xiulan   

  1. Beiman Special Steel Co Ltd,Dongbei Special Steel Group,Qiqiha'er 161041
  • Online:2008-04-01 Published:2023-01-20

90 t电弧炉-LF(VD)-连铸-连轧流程生产链轨节钢35MnBM的工艺实践

朱志欣 李  艾  王秀兰   

  1. 东北特钢集团北满特殊钢有限责任公司,齐齐哈尔161041
  • 作者简介:朱志欣(1967-),男,工程师,1990年本溪冶金专科学校毕 业,产品开发及冶炼工艺研究

Abstract: The   φ65,φ70   mm  products   of  caterpillar   track   steel   35MnBM(0.35C,1.25Mn,0.0018B,0.029Al, 0.09V)was produced by  90 t  electric  arc  fumace-LF(VD)refining  -240 mm×240 mm billet  concasting  -  continuous rolling process at Beiman Special Steel. With VD treatment and whole period shield casting practice the[N] was ≤78×  10-6,the rating of non- metallic inclusions in steel was 0~2,no hair crack was detected and the grain size, structure and hardenability of steel all met the requirement of standard

Key words: EAF-LF(VD)-CC-CR Flow Sheet,Caterpillar Track Steel 35MnBM,Process Practice

摘要: 北满特钢通过90 t电弧炉-LF(VD)精炼-240 mm×240 mm方坯连铸-连轧工艺生产④65、φ70 mm链 轨节钢35MnBM(%:0.35C、1.25Mn,0.0018B、0.029Al,0.09V)。通过VD处理和全程无氧化保护浇铸,使[N]≤ 78×10-6,钢中非金属夹杂物为0~2级,无发纹,晶粒度、组织和淬透性均满足标准要求。

关键词: EAF-LF(VD)-CC-CR流程链轨节钢35MnBM ,  , 工艺实践