Optimization of Process for Hollow Forgings of ESR Alloy Steels

Zhao Xin1, Liu Defu2   

  1. 1  The  Sixth  Department,Zhengzhou  Institute  of Aeronautic  Industry  Management,Zhengzhou  450015;
    2  Northeast  Special  Steel  Croup  Co  Ltd,Dalian  116031
  • Received:2008-01-19 Online:2008-08-01 Published:2022-12-23

电渣合金钢空心类锻件生产工艺的优化

赵 新 1,  刘德富2   

  1. 1郑州航空工业管理学院六系,郑州450015;
    2东北特殊钢集团有限公司,大连116031
  • 作者简介:赵 新(1969-),男,博士,副教授,1991年东北重型机械学院毕业,难变形Fe-C合金的塑性加工。
  • 基金资助:
    国 家 自 然 科 学 基 金 钢 铁 联 合 基 金 项 目 资 助 (50271060,50371074)

Abstract: Typical hollow forgings-electro-slag remelting (ESR)alloy steel roll sleeve with inner diameter 560~880 mm, outer diameter 670~1200 mm and length 1300~1780 mm is usually produced by ≥2 t ingots. Based on the ensuring product quality, as compared with traditional forging process, it is available to decrease by 2 procedures and once re- heating with using optimized process- direct forging upsetting. The forgings yield increased by 5%~15% to obviously de- crease production cost.

摘要: 典型的空心锻件-电渣合金钢辊套锭重≥2 t,内孔直径560~880 mm,外径670~1200 mm,长1300~1780 mm。在保证质量的基础上,采用改进的工艺-直接锻粗法后,与传统工艺相比,可减少2道工序和一次中间加热,锻件成材率提高5%~15%,显著降低生产成本。

关键词: 空心类锻件, 电渣重熔, 合金钢, , 锻造, , 成材率