Optimization of Parameters for High Efficiency RH Decarburization Process

Liu Baisong1,2, Zhu Guosen2, Li Benhai2, Zhu Lixin2, Cui Aimin3, Li Huanxi1   

  1. 1 School of Materia] Science and Engineering, Beihang University, Beijing 100083;
    2Shongang Research Institute of Technology, Beijing 100041 ;
    3Qianan Iron and Steel Co, Shougang, Qianan 064404
  • Received:2008-07-21 Online:2009-02-01 Published:2022-11-29

高效RH脱碳工艺参数的优化

刘柏松1,2, 朱国森2, 李本海2, 朱立新2, 崔爱民3, 李焕喜1   

  1. 1北京航空航天大学材料科学与工程学院,北京100083;
    2首钢技术研究院,北京100041 ;
    3首钢迁钢公司,迁安064404
  • 作者简介:刘柏松(1979-),女,博士研究生,从事纯净钢的生产研究.

Abstract: Based on(lecarburizah(m math model for RH process, the decarburization behavior of a 210 t RH unit has been studied to analyze the effect of vacuum, lifting gas flow rate and up-leg inner diameter on decarburizing process. At condition of natural decarburization, according to results of sampling analysis to calculate de('arburization rate constant Kc, it was found that the whole (lecarburization process was divided into two phases: quick decarburization phase ami decarburization stagnated phase. The results showed that with increasing vacuum, the decarburizing rate increased and end [C] decreased ;with increasing gas flow rate the increase of decarburizing rate was not outstanding; using suitable up-leg imier diameter was available to get larger decarburizing rate ; and the decarburizing rate constant could be up to 0. 287 min-1 at quick dec'arburization phase.

Key words: Decarburizing Rate, RH Refining, ULC Steel

摘要: 基于RH脱碳数学模型,研究了210tRH精炼装置的脱碳行为,分析了真空度、提升气体流量及浸渍管内径等因素对脱碳过程的影响;在自然脱碳条件下,根据实际取样分析结果,计算出脱碳速率常数KC,发现整个脱碳过程分为两个阶段,即快速脱碳阶段和脱碳停滞阶段。提高真空度可提高脱碳速率和降低终点[C];提高气体流量不能显著提高脱碳速率,应选择合适的浸渍管内径;快速脱碳阶段的脱碳速率常数可达0.287min-1

关键词: 脱碳速率, RH精炼, 超低碳钢