Operational Development of φ210 mm Bar Products by 800 Blooming Mill

Sun Dongshen , Yu Li   

  1. Special Steel Works,Plate Co Ltd,Benxi lron and Steel Group, Benxi117000)
  • Received:2009-02-26 Online:2009-08-01 Published:2022-12-20

800初轧机轧制Φ210mm棒材的开发实践

孙东升,于  莉   

  1. 本钢板材股份有限公司特殊钢厂,本溪117000
  • 作者简介:孙东升(1965-),男,高级工程师,本钢特钢厂厂长,1986年东北大学毕业,特殊钢产品冶炼与轧制的研究。

Abstract: With round- large oval- box- flat box pass system to replace original round- flat- octagon- flat box pass system,and optimized reduction schedule to roll φ210 mm carbon and alloy steel bars from 350 mm×470 mm bloom by 800 blooming mill at Special Steel Works, Bensteel, the qualified rate of rolled steel products was up to 99.75%.

Key words:  , φ210 mm Steel Bar,Pass Design,Reduction Schedule

摘要: 通过本钢特钢厂800初轧机将350mm×470mm碳素和合金钢坯轧制成Φ210mm棒材的孔型由圆-大椭圆-箱-平箱系统替代原有的圆-扁八角-平箱系统,并优化压下制度,使轧制的合格率达99.75%。