ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2009, Vol. 30 ›› Issue (5): 19-21.

Previous Articles     Next Articles

Influence of Nozzles Blocking of RH Up-Snorkel on Circulation Flow Rate

Ai Xingang , Bao Yanping , Yue  Feng , Cui  Heng  ,  Wu  Huajie   

  1. School of Metallurgical and Ecological Engineering,University of Science and Technology,Beijing 100083
  • Received:2009-04-09 Online:2009-10-01 Published:2022-11-21

RH上升管吹气孔堵塞对循环流量的影响

艾新港,包燕平,岳  峰,崔  衡,吴华杰   

  1. 北京科技大学冶金与生态工程学院,北京 100083
  • 作者简介:艾新港(1978-),男,博士生,二次精炼研究。
  • 基金资助:
    “十一五”国家科技支撑计划课题(2006BAE03A06)

Abstract: In order to study the influence of nozzles blocking of a 210 t RH unit up-snorkel on circulation flow rate, the 1:4 water model test has been carried out. Results show that with numbers of blocking nozzles in sequence being more than 3,the circulation flow rate decreases obviously; as the number of blocking nozzles is same,the decrease of circulation flow rate with blocking nozales in symmetry is less than that with blocking nozzles in sequence; RH process could be normalcontinuous as the numbers of blocking nozzles are 3 or less than 3;and with lowing the location of nozzles the circulation flow rate increases markedlv.

Key words: RH Refining, Nozzles Blocking, Circulation Flow Rate, Water Model

摘要: 为研究210 t RH上升管吹气孔堵塞对循环流量的影响,进行了1:4水模型试验。结果表明,顺次堵吹气孔3个以上时,循环流量明显降低;堵塞吹气孔数量相同时,对称堵吹气孔对循环流量的减少小于顺次堵吹气孔,堵吹气孔3个和3个以下时可以正常生产;降低吹气孔的位置可以显著提高循环流量。