ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2009, Vol. 30 ›› Issue (6): 47-48.

Previous Articles     Next Articles

Development of Forged Bar of Steel X10 CrNiMoV12-2-2 for Turbine Blade

Wu Jiangfeng, Chen Xinjian ,Zhang Fufei   

  1. Special Steel Branch, Baoshan Iron & Steel Co Ltd, Shanghai 200940
  • Received:2009-05-06 Online:2009-12-01 Published:2022-11-29

汽轮机叶片用钢X10CrNiMoV12-2-2锻造棒材的开发

吴江枫,陈新建,张甫飞   

  1. 宝山钢铁股份有限公司特殊钢分公司,上海200940
  • 作者简介:吴江枫(1953-),男,工程师,1987年吴淞大学毕业,特殊钢新材料开发。

Abstract: Steel for Turbine Blade, X10CrNiMoV12-2-2, Forged Product

Key words: Steel for Turbine Blade, X10CrNiMoV12-2-2, Forged Product

摘要: X10CrNiMoV12-2-2钢(%:0.08~0.13C、11.4~12.5Cr、2.2~2.8Ni、1.6~1.8Mo、0.25~0.40V、0.020~0.040N)经20 t EAF-AOD-LF冶炼后铸成Φ490 mm电极,电渣重熔成Φ600 mm钢锭,锻造成Φ180~240mm棒材。检验结果表明,钢中有害元素Sb为0.002%,As 0.010%,Sn 0.010%,其夹杂物级别、晶粒度、力学性能、FATT(脆性转变温度)、晶间断裂百分比、δ-自由铁素体含量均达到技术标准要求。

关键词: 汽轮机叶片用钢, X10CrNiMoV12-2-2, 锻材