A Study on Smelting Process of Ultra-pure Austenite Stainless Steel 005Cr25Ni20

Guo Shujuan1 ,Han Tao2   

  1. 1 College of Professional Technology, Liaoning University of Petroleum and Chemical Technology, Fushun 113001 ;
    2 Technology Center, Fushun Special Steel Co, Fushun 113001
  • Received:2011-03-11 Online:2011-08-01 Published:2022-11-03

超纯奥氏体不锈钢005Cr25Ni20冶炼工艺研究

郭淑娟1,韩涛2   

  1. 1辽宁石油化工大学职业技术学院,抚顺113001:
    2抚顺特钢技术中心,抚顺113001
  • 作者简介:郭淑娟(1972-),女,硕士,讲师,工程师,大连交通大学毕业,金属材料研究。

Abstract:  As the requirement for included element C, P, S and Si content in ultra-pure austenite steel 005Cr25Ni20 (% :24 ~26Cr, 19 〜22Ni) are very low i. e. (%) :≤0. 010C, ≤0. 010S, ≤0. 010P and W≤0. 15 Si, the steel is smelted by 3 t vacuum induction furnace 4- vacuum consumption remelting furnace steelmaking process. With using quality pure iron (% : 0. 009C, 0. 035Si, 0. 001 2S, 0. 004 5P), high pure chromium iron (%: 0. 010 - 0. 021C, 0. 11 - 0. 13Si, 0. 002 5 ~0. 005 OS, 0. 001 5 ~0. 005 OP) and Ni-plate (Ni399%), adding Al, metal Ca, Ni-Mg for deoxidation during vacuum induction smelting, and whole process computer control vacuum consumption remelting speed, the chemical composition of finished products of steel is (% :) 0. 005 〜0.007C, 0. 33 〜0. 34Mn, 0. 03 -0. 04Si, 0. 001 〜0.002S, 0. 004 〜 0. 005P, 24. 34 〜24. 62Cr, 21. 20 〜21.25Ni to meet the technical requirement, and the oxygen content in steel- (12 ~ 22) x 10-6 is lower than in steel by ESR process- (30 ~ 80) x 10-6.

Key words:  , Ultra-pure Austenite Stainless Steel 005Cr25Ni20, Vacuum Induction Furnace. Vacuum Consumption Remelting Furnace, Smelting Process

摘要: 005Cr25Ni20钢(%:24~26Cr、19~22Ni)要求C、P、S、Si等杂质元素含量低-(%):≤0.010C、≤0.010S、≤0.010P、≤0.15Si,因此采用3 t真空感应炉+真空自耗重熔炉冶炼工艺。通过采用优质纯铁(%:0.009C、0.035Si、0.001 2S、0.004 5P)、高纯铬铁(%:0.010~0.021C、0.11~0.13Si、0.002 5~0.005 0S、0.001 5~0.005 0P)和Ni板(Ni≥99%),真空感应炉熔炼时加A1、金属Ca、Ni-Mg脱氧,全程计算机控制真空自耗重熔速度,该钢成品化学成分为(%):0.005~0.007C、0.33~0.34Mn、0.03~0.04Si、0.001~0.002S、0.004~0.005P、24.34~24.62Cr、21.20~21.25Ni,达到技术要求,钢中氧含量为(12~22)×10-6,低于电渣重熔钢的氧含量-(30~80)×10-6