Analysis of Mathematical Simulation on Tundish for Billet Caster at Shougang

Ding Ning1,2 , Bao Yanping1  , Chen Jingsheng2 , Cui Jingyu2 , Sun Qisong2 , Wang Lifeng2   

  1. 1. School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083 ;
    2. Research Institute of Technology, Shougang, Beijing 100043 ;
  • Received:2011-04-06 Online:2011-10-01 Published:2022-10-29

首钢小方坯连铸机中间包数值模拟分析

丁宁1,2,包燕平1,陈京生2,崔京玉2,孙齐松2,王立峰2   

  1. 1. 北京科技大学冶金与生态工程学院.北京 100083;
    2. 首钢技术研究院,北京 100043 ;
  • 作者简介:丁 宁(1979-),男,硕士,工程师,2007年东北大学毕业,品种钢开发和研究

Abstract: A mathematical model for 14. 5 t tundish casting 160 mm x 160 mm billet at Shougang is established and the numerical calculation of flow and temperature of liquid in shape tundish for 4-strand is calculated by using fluid dynamic software Fluent to get the flow speed field, temperature field and residence time distribution curves of liquid in tundish. Calculation results show that the maximum temperature difference between each strand is 8 K, therefore the lower overheating extent liquid shall be avoided; besides the percentage of dead volume of No l strand is 20% little larger than that other strands ( 10% 〜12% ) , the flow parameters of liquid in tundish meet the requirement for casting operation.

Key words: 160 mm X 160 mm Casting Billet, Tundish, Mathematic Simulation, Residence Time Distribution Curves, Temperature Field

摘要: 针对首钢160 mm×160 mm方坯连铸机14.5 t中间包建立数学模型,采用流体力学计算软件Fluent对4流异型中间包内钢液流动和温度进行了数值计算,得出中间包钢液流动的速度场、温度场和停留时间分布曲线。计算结果表明,各流最大温度差为8 K,应避免低过热度浇铸;1流死区体积分率为20%略大于其余各流(10%~20%)外,中间包钢水流动参数可以满足生产的需要。

关键词: 160mm×160mm铸坯, 中间包, 数值模拟, 停留时间分布曲线, 温度场