Study and Application of BOF Steelmaking Steel Bearing Molybdenum by Molybdenum Trioxide to Replace Ferromolybdenum

Li Yongchao1,2, Yan Lizhen1, Ji Dandan1, Huo Zhibin1   

  1. 1 Xingtai Iron and Steel Co Ltd, Xingtai 054027 ;
    2 Hebei Engineering Research Center for Wire and Rod, Xingtai 054027
  • Received:2016-12-10 Online:2017-06-01 Published:2022-07-21

三氧化钼替代钼铁转炉冶炼含钼钢的研究和应用

李永超1,2,阎丽珍1,姬旦旦1,霍志斌1   

  1. 1邢台钢铁有限责任公司,邢台054027;
    2河北省线材工程技术研究中心,邢台054027
  • 作者简介:李永超(1985-),男,硕士(2012年北京科技大学),工程师,2009年河北理工大学(本科)毕业,中低碳冷镦钢的开发和工艺控制。

Abstract: The conditions of thermodynamics and kinetics for molybdenum trioxide reduced by main elements C, Si, Mn and Fe in BOF liquid are analyzed and the adding method of molybdenum trioxide during BOF steelmaking process is discussed. And the commercial production of steelmaking medium carbon cold-heading steel SCM435 (/%:0.35C, 0.22Si, 0.67Mn, 0.003S, 0.012P, 0.97Cr, 0.20Mo) is carried out in an 80t BOF by molybdenum trioxide to replace ferromolybdenum. Results show that the molybdenum trioxide in BOF has excellent reduction condition;in order to prevent evaporation of molybdenum trioxide, it is adding mix with inhibitor lime to insure the yield of molybdenum. The commercial pilot production show that by using molybdenum trioxide the average yield o£ molybdenum is up to 96.65% , the cost of tonnage steel decreases by 5.1 yuan, it meets the requirement of production.

Key words: Molybdenum Trioxide to Replace Ferromolybdenum, Reduction, 80t BOF, Analysis on Thermodynamics, Application

摘要: 分析了转炉钢水中主要元素(C、Si、Mn、Fe)还原三氧化钼的热力学和动力学条件,讨论了转炉冶炼过程中三氧化钼的加入方式。并在80t转炉用三氧化钼替代钼铁进行冶炼中碳冷镦钢SCM435(/%:0.35C,0.22Si,0.67Mn,0.003S,0.012P,0.97Cr,0.20Mo)的工业实践。结果表明,三氧化钼在转炉中具有良好的还原条件;为防止三氧化钼挥发,其应与抑制剂CaO混合加入以保证钼的收得率。工业试验结果表明,钼的平均收得率达到96.65%,吨钢成本降低5.1元,满足生产需求。

关键词: 三氧化钼替代钼铁, 还原, 80t转炉, 热力学分析, 应用