Production Practice of Ultra Deep Desulphurization of Steel GCrl5 by 80 t BOF-LF-RH Process

Zhao Shijie1,2, Xuan Zhenbo3 , Feng Wenfu1,2, Liu Xueqiang1,2, Fan Jianying1,2 , Huo Liguo1,2   

  1. 1 Steelmaking Plant, Xingtai Iron & Steel Corp . Ltd,Xingtai 054027 ;
    2 Heibei Engineering Research Center for Wire and Rod, Xingtai 054027;
    3 Tianjin Metallurgical Group No. 3 Steel Rolling Co Ltd, Tianjin 301606)
  • Received:2020-04-28 Online:2020-10-01 Published:2022-05-05

80 t BOF-LF-RH流程GCrl5钢超深脱硫的生产实践

赵世杰1,2,轩振博3, 冯文甫1,2, 刘学强1,2, 范建英1,2, 霍立国1,2   

  1. 1邢台钢铁有限责任公司炼钢厂,邢台054027;
    2河北省线材工程技术研究中心,邢台054027 ;
    3天津冶金集团轧)钢铁有限公司,天津301606
  • 作者简介:赵世杰(1985-),男,工程师,内蒙古工业大学(本科)毕业, 炼钢技术研究。

Abstract: Through the practice show that, it can be seen the production of bearing steel, the converter tapping temperature ≥1650℃, tapping oxygen ≤300 x 10-6, and 18 kg/t slag can achieve 50% desulfurization efficiency in the tapping process. At the same time, the mode of u slag retaining cone + slide plate slag retaining" is adopted in converter tapping to reduce sulfur by another 0. 000 5% ; the mode of aluminum adding in BOF tapping + LF refining to deoxidize with ferrosilicon powder and controlling the binary basicity of slag to be 5 ~ 6 can achieve more than 50% desulfurization effect and stabilize the casting performance to get finished product sulfur content ≤0.0015% .

Key words:  , Bearing Steel, Desulphurization, Refine, Production Practice

摘要: 通过实践表明,生产轴承钢时,转炉出钢温度≥1650℃、出钢[0]≤300×10-6,18 kg/t的渣料可实现出钢过程50%的脱硫效率;同时,转炉出钢采用"挡渣锥+滑板挡渣"双挡的模式,实现将硫再降低0.0005%;采取"铝在转炉出钢时加入+LF精炼使用硅铁粉脱氧"模式,以及控制炉渣二元碱度在5~6,可实现50%以上的脱硫效率的同时,也能够稳定浇铸性能,达到成品硫≤0.0015%。