ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2021, Vol. 42 ›› Issue (2): 75-77.

Previous Articles    

Development and Performance of Hot Rolled Enamel Steel for Water Heater Tank

Wang Yan,He Jin ,Xin Jianqing   

  1. Technical Center,Shanxi Taigang Stainless Steel Co Ltd,Taiyuan 030003
  • Received:2020-09-10 Online:2021-04-01 Published:2022-04-18

热水器内胆用热轧搪瓷钢的开发与性能

王艳,何晋,辛建卿
  

  1. 山西太钢不锈钢股份有限公司技术中心,太原030003
  • 作者简介:王 艳(1982-),女,硕士(2011年内蒙古科技大学),工程师,热轧钢带产品开发。

Abstract: With the process measures including composition controlling by 180 t LD with top-bottom blowing and Ti microalloying by LF, continuous casting into 230 mm slabs and heating at 1200 ~ 1250℃, rapid cooling after controlled rolling, coiling at 500 ~700 ℃ ,Shanxi Taigang Stainless Steel Co Ltd has successfully developed 2 mm hot-rolled enamel steel sheet for water heater tank (/% : ≤0.14C, ≤1.20Mn. ≤0.030P,≤0.025S ,≤0.l0Ti). The results show that the steel sheet after simulated enamelling at 850 ℃ for 10 min still has high strength (Rm 366 MPa) and good formability ;the hot-rolled grain is uniform and fine, and there is no obvious change in grain size after enamel, and there are a large number of second phase particles dispersed precipitation ; for commercial produced enamel steel after single-sided enamel ,it shows good scale explosion resistance and can meet the application requirements of making water heater tank.

Key words: Water Heater Tank, Hot-Rolled, Enamel Steel, Precipitated Phase ,

摘要: 通过180 t顶底复吹转炉+LF成分控制及Ti微合金化,连铸成230 mm板坯经1200-1250℃加热,控制轧制后快速冷却至500~700℃卷取等工艺措施,山西太钢不锈钢公司成功开发了热水器内胆用热轧搪瓷钢(/%:≤0.14C,≤0.06Si,≤1.20Mn,≤0.030P,≤0.025S,≤0.10Ti)2 mm热轧钢板。结果表明,热轧钢板经850℃10 min模拟搪烧后仍具有较高的强度(Rm 366 MPa)以及良好的成型性能;热轧态晶粒均匀细小,搪烧后晶粒尺寸无明显变化,且有大量第二相粒子弥散析出;工业生产的搪瓷钢经单面搪瓷后表现出良好的抗鳞爆性能;能够满足制作热水器内胆的各项应用要求。