Cause Analysis on Surface Crack of Drill Steel 55SiMnMo Rolling Product and Process Improvement

Zhao Jingcun, Zhu Ye   

  1. Zhao Jingcun, Zhu Ye
  • Online:2023-02-01 Published:2023-01-30

钎具钢55SiMnMo轧材表面裂纹的成因分析及工艺改进

赵景存,朱 叶   

  1. (石钢京诚装备技术有限公司,营口115000)

  • 作者简介:赵景存(1985-),男,工程师; E-mail:404262432@q4.com; 收稿日期:2022-08-10

Abstract: The  surface of rolled products of drill  steel  55SiMnMo produced by  100 t BOF-LF-VD-4450 mm CC bloom- φ200 mm rolling bar production process is prone to  surface crack.The effect of superheat,secondary cooling,casting  speed and  composition(Ti.B)on  defects  are  analyzed  and  compared.  Through  process  improvement  which  is  obtained  that  by controlling      superheat      20-30      ℃,B      content      controlled≤0.0008%,Ti      content      0.015%-0.025%,drawing      speed 0.41  m/min,and  secondary  cooling  ratio  0.17  L/kg,the  crack  defect  rate  decreases  from   12.2%  to1.6%.

Key words: 55SiMnMo , Drill , Steel, Surface , Crack, Proess , Improvement

摘要: 针对100 t BOF-LF-VD-Φ450 mm连铸坯-Φ200 mm轧材流程生产的钎具钢55SiMnMo轧材表面易产生裂纹缺陷,分析对比了过热度、二次冷却、拉速、成分(Ti.B)等对缺陷的影响。通过工艺改进;控制钢水过热度20~30℃,控制B含量≤0.0008%,加Ti 0.015%~0.025%,拉速0.41 m/min,二冷比水量0.17 L/kg,使裂纹的缺陷率由原来的12.2%降低到1.6%。

关键词: 55SiMnMo钎具钢, 表面裂纹, 工艺改进