[1] |
Meng Qingyong, Shan Qinglin, Pan Hongwei, Lu Boxun, Shi Xiaowei, Wen Juwen.
High-temperature Thermoplastic Analysis on High-chromium Weathering Resistant Steel Q350EW
[J]. Special Steel, 2024, 45(6): 23-27.
|
[2] |
Zhang Yanmei, Yu Haicun, Qiu Qiuling.
Effect of Solid Solution Process on the Organization and Mechanical Properties of 3Al-310S Heat-resistant Steel
[J]. Special Steel, 2024, 45(6): 95-101.
|
[3] |
Ni Zhuowen, Zhu Hongchun, Li Huabing, Jiang Zhouhua, Sun Zhengxin, He Zhiyu.
Analysis of the Types and Distribution of Inclusions in H13 Die Steel Electroslag Ingots
[J]. Special Steel, 2024, 45(6): 48-52.
|
[4] |
Liu Junkai, Yu Yipeng, Zhang Jinglin, Zhang Jiansheng, Zhang Jianfu.
The Influence of Deformation and Heating Temperature on the Impact Toughness of 2205 Duplex Stainless Steel
[J]. Special Steel, 2024, 45(6): 69-72.
|
[5] |
Peng Feng, Li Xu, Li Bopeng, Zhang Yue, Wang Zhanzhong, Guo Shibei.
Development of 10.9 Grade 32CrB4 Quenched and Tempered Round Steel for Fasteners
[J]. Special Steel, 2024, 45(6): 8-11.
|
[6] |
Zhao Jiawei, Tian Jialong, Yang Ping, Zhan Dongping, Jiang Zhouhua.
Effect of Dual-aging Process on Microstructure and Properties of Co-precipitation Hardening Ultra-high Strength Steel
[J]. Special Steel, 2024, 45(6): 88-94.
|
[7] |
Zhao Bo, Wang Shanbao, Xie Degang, Yuan Qin, Ai Fangfang, Wang Xixiang, Guo Jinmei.
Microstructure and Properties of Seamless Steel Pipe Gr.6 after Rolling and Normalizing
[J]. Special Steel, 2024, 45(6): 102-107.
|
[8] |
Zhang Xingli, Qi Fengyou, Su Yongze, Cui Guibo, Tang Qing, Hou Jianwei.
Ractice of EF3 Ultra-low Phosphorus Smelting Process for High-grade Pipeline Welding Wire
[J]. Special Steel, 2024, 45(6): 57-61.
|
[9] |
Chen Jun, Peng Guangjian, Lin Dan, Huang Zhenhua.
Production Practice of Ultra-Low Carbon Steel H1T in 150 mm×150 mm Small Billet
[J]. Special Steel, 2024, 45(6): 17-22.
|
[10] |
Wang Li, Liu Chengbao, Li Haoqiu, Wang Yi, Sun Zonghui, Liu Chunwei, Yang Chaoyun, Fu Zhihao.
Effect of Rare Earth on Inclusions and Fatigue Properties of 20CrMnTi Gear Steel
[J]. Special Steel, 2024, 45(6): 117-124.
|
[11] |
Yang Wenbin, Liu Zhongqiu, Wang Fang, Huang Xuechi, Lang Yuping, Li Baokuan.
Effect of Melting Rate on Solidification Process of High Filled Ratio 06Cr18Ni11Ti Electroslag Remelting Ingot
[J]. Special Steel, 2024, 45(6): 28-36.
|
[12] |
Xie Kang, Mo Jinqiang, Zhang Wei, Wang Lijun.
The Effect and Control of Rare Earth Ce on Carbonitrides Precipitation in 441 Ferritic Stainless Steel
[J]. Special Steel, 2024, 45(6): 1-7.
|
[13] |
Sun Jian, Liu Zhanli, Li Jie, Zhang Pengfei, Zheng Jinghui, Xing Liyong.
High Temperture Thermoplastic Behavior of BTW1 Steel Continuous Casting Slab
[J]. Special Steel, 2024, 45(6): 12-16.
|
[14] |
Zheng Anmin, Fan Xuanyu, Huang Zengxin, Mao Wangwang, Yu Yanchong, Zhang Jinling, Wang Shebin.
Effect of Rare Earth Ce on the Evolution of Inclusions in 20MnTiB Cold Heading Steel
[J]. Special Steel, 2024, 45(6): 37-47.
|
[15] |
Zhao Guangdi, Zang Ximin, Liu Zhichao, Jing Yu'an.
Influence of Quenching Process on the Microstructure Evolution and Hardness of A514CrQ Rack Steel
[J]. Special Steel, 2024, 45(6): 73-82.
|