Special Steel ›› 2009, Vol. 30 ›› Issue (4): 63-65.

Previous Articles     Next Articles

Effect of Austempering Isothermal-Time at Bainite Field on Structure and Mechanical Properties of Low Silicon TRIP Steel

Jing Cainian1, Chen Xiaohui2, Liu Zaixue1, Tan Qizhong1, Li Liang1   

  1. 1 School of Materials Science and  Engineering,Shandong  Architecture  University,Jinan  250101;
    2 Lab of Mechanical Manufacture, Shandong  Jiaotong  University, Jinan 250023
  • Received:2009-01-12 Online:2009-08-01 Published:2022-12-20

贝氏体区等温时间对低硅TRIP钢组织和力学性能的影响

景财年1, 陈晓辉2, 刘在学1, 谭启忠1, 李  亮1   

  1. 1山东建筑大学材料科学与工程学院,济南250101;
    2山东交通学院机械加工实验中心,济南250023
  • 作者简介:景财年(1973-),男,博士,副教授,钢铁材料组织和性能研究。
  • 基金资助:
    山 东 省 博 士 后 创 新 项 目 (20070225),
    建设部科技计 划项目(2008-K4-7),
    山东省 博士基金(2008BS04023)

Abstract: Structure  and  mechanical  properties  of0. 15C- 1.5Mn- 1.5Al-0.3Si  TRIP  steel  heated  at  820  ℃  for  2  min then quenching  in  450  ℃  salt bath  for  5~300  s,air  cooling  have  been  studied.  Results  showed  that  with  increasing  iso- thermal-time  in  Bainite  transformation  field  at  450  ℃,the  yield  strength  and  elongation  of steel  increased  while  tensile strength  decreased, and  the  product  of tensile  strength-elongation  of  steel  was  highest  i.e.23000  MPa%  with  isothermal- treating  for  60  s; as  isothermal-treating  for  less  than  60  s, with  increasing  isothermal-treating  time, the  retained  austenite content  in  steel  increased, as  isothermal-treating  for  more  than  60  s, with  increasing  isothermal-treating  time, the  retained austenite content in  steel decreased, and the retained austenite content in  steel isothermal-treating for 60  s was highest i.e.  14%.

摘要: 研究了0.15C-1.5Mn-1.5Al-0.3Si TRIP钢820℃2 min加热后快冷至450℃盐浴中保温5~300s空冷的组织和力学性能。结果表明,随在贝氏体转变区450℃等温时间的增加,该钢的屈服强度和伸长率增加,抗拉强度降低,等温时间60s时强塑积最佳,为23 000MPa%;等温时间≤60s时随等温时间增加钢中残余奥氏体含量增加,>60s时随等温时间的增加钢中残余奥氏体含量降低,60s时钢中残余奥氏体达到最高值,为14%。