Production of Steel Plate for Wheel Spoke by Controlled Rolling and Cooling Technology

Ma  Haitao1,2, Wu  Di1, Zhang  Yongfu3   

  1. 1 The State Key Lab of Rolling Technology and Automation,Northeasterm University,Shenyang 110004;
    2 Dept of Metallurgical Engineering,Liaoning Institute of Science and Technology,Benxi 117022;
    3 Technology Center,Benxi Iron and Steel(Group)Co Ltd,Benxi117000
  • Received:2008-01-07 Online:2008-08-01 Published:2022-12-23

采用控轧控冷工艺生产车轮用轮辐钢板

马海涛1,2, 吴  迪1, 张永富3   

  1. 1东北大学轧制技术及连轧自动化国家重点实验室,沈阳110004;
    2辽宁科技学院冶金工程系,本溪117022;
    3本溪钢铁(集团)公司技术中心,本溪117000
  • 作者简介:马海涛(1969-),男,博士生,副教授,高级工程师,1992年东北大学毕业,材料加工工程。
  • 基金资助:
    国家自然科学基金资助项目(50334010)

Abstract:  Rolling        test        on        steel        plate(0.09C,0. 12Si,0.98Mn,0.010P,0.005S,0.010Nb,0.04Als)for        wheel spoke  with  finishing  rolling  temperature  830~890  ℃  and  coiling  temperature  620~680  ℃  has  been  carried  out  by 1700mm  hot  rolling  mill  train.  Results  showed  that  with  slab  heating  temperature  1230~1250  ℃,finishing  rolling  tem- perature  870±15℃,coiling  temperature  660±15  ℃,the  structure  of  steel  plate  for  wheel  spoke  was  fine  ferrite  +  minor pearlite,the   yield   strength   of   steel   was   335~380MPa,tensile   strength   430~485MPa,elongation   26%~31%,the   longitudinal  strength  difference  of each  steel  coil  was  13~37MPa,and  the  punching  formability  during  vehicle  wheel  manufacturing  was  excellent  with  punching  rejection  rate  less  than  0.3%.

摘要: 通过1700 mm热连轧机组对轮辐钢(%:0.09C、0.12Si、0.98Mn、0.010P、0.005S、0.010Nb、0.04Als)进行830~890℃终轧温度和620~680℃卷取温度的轧制试验。结果表明,板坯加热温度1230~1250℃、终轧温度(870±15)℃、卷取温度(660±15)℃生产的车轮用轮辐钢板的组织为细铁素体加少量的珠光体,屈服强度335~380 MPa,抗拉强度430~485 MPa,伸长率26%~31%,每卷带钢的纵向强度差为13~37 MPa,在车轮制作过程中冲压成型良好,冲废率小于0.3%。