Abstract: The φ140~170 mm bars of steel 37CrMnMo(0.35~0.38C,0.85~1.00Mn,0.90~1.20Cr,0.28~ 0.33Mo,≤0.015P,≤0.008S)for coupling sleeve of petroleum drill stem are produced by 50t EBT arc furnace-LF (VD)-Al and Ca-Si wire feeding-3.16 t ingot casting-800/650×4 mills rolling flow sheet at Benxi steel. Analyais and examination results showed that hydrogen content in steel products was (0.5~1)×10-6,oxygen content(8~20)×10-6,nitrogen content(55~90)×10-6,inclusion rating 0~2, J25 hardenability HRC value 42~51, transversal impact energy at - 10℃ 56~218J, longitudinal impact energy at - 10℃ 76~233 J and the strength and plasticity of products all met the requirement of standard.
Key words: Steel 37CrMnMo,LF(VD),Wire Feeding,Mechanical Properties
摘要: 本钢采用50 t偏心底电弧炉熔炼-LF(VD)-喂Al和Ca-Si线-3.16 t铸锭-800/650×4轧机流程生产Φ140~170 mm石油钻杆连接套用37CrMnMo钢(%:0.35~0.38C、0.85~1.00Mn、0.90~1.20Cr、0.28~0.33Mo、≤0.015P、≤0.008S)。检验结果表明,钢材中H含量(0.5~1)×10-6,O含量(8~20)×10-6,N含量(55~90)×10-6,夹杂物0~2级,J25淬透性HRC值42~51,-10℃横向冲击功56~218 J,-10℃纵向冲击功76~233 J,强度和塑性均满足标准要求。
关键词: 37CrMnMo钢, LF(VD) , , 喂丝 , 力学性能
Zhao Qianshui , Sui Lingyun. Production Practice of Steel 37CrMnMo for Coupling Sleeve of Petroleum Drill Stem[J]. Special Steel, 2007, 28(3): 66-67.
赵千水, 隋玲云. 石油钻杆连接套用37CrMnMo钢的生产实践[J]. 特殊钢, 2007, 28(3): 66-67.
Add to citation manager EndNote|Ris|BibTeX
URL: https://www.specialsteeljournal.com/EN/
https://www.specialsteeljournal.com/EN/Y2007/V28/I3/66