Experiment on Calcined Denitriding Process of Recarburizer

Sun Yaqin,Chen Qizhong,Zhang Zhuo and Jin Minglin   

  1. Department of Material Engineering,Shanghai Institute of Technology, Shanghai 200233
  • Received:2006-04-19 Online:2006-10-01 Published:2023-03-28

增碳剂煅烧脱氮工艺实验研究

孙亚琴, 陈麒忠, 张 琢, 金鸣林   

  1. 上海应用技术学院材料工程系,上海200233
  • 作者简介:孙亚琴(1966-),女,讲师,1995年上海大学毕业,从事炼 钢及连铸工艺研究。

Abstract: The experiment on calcined denitriding process of recarburizer 95(containing 0. 10%N),petroleum coke(0.93%N)and pitch coke(0.40% N)has been carried out. The results indicated that with increasing cal- cined temperature the nitrogen content in 3 kinds of recarburizer decreased and as the temperature was more than 2000℃,the nitrogen content in each recarburizer was less than 100×10-6.As calcined temperature was 1800℃, the nitrogen content in recarburizer 95 was less than 300×10-6 while that in petroleum coke or pitch coke was less than 100×10-6.

摘要: 对95增碳剂(0.10%N)、石油焦(0.93%N)和沥青焦(0.40%N)进行煅烧脱氮试验,试验结果 表明:随煅烧温度的提高,3种增碳剂中的氮含量都下降,温度大于2000 ℃时,各增碳剂中的氮含量均小于 100×10-6 。1800℃煅烧时,95增碳剂的氮含量小于300×10-6,石油焦或沥青焦的氮含量小于100×10-6