Effect of Deforming Temperature on Structure and Properties of Spring Steel 55SiCrA
更新时间:2026-01-21
    • Effect of Deforming Temperature on Structure and Properties of Spring Steel 55SiCrA

    • Special Steel   Vol. 31, Issue 2, Pages: 60-62(2010)
    • Received:28 September 2009,

      Online First:17 November 2022,

      Published:17 November 2010

    移动端阅览

  • 肖金福, 刘雅政, 孙小军, et al. Effect of Deforming Temperature on Structure and Properties of Spring Steel 55SiCrA[J]. Special Steel, 2010, 31(2): 60-62. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Deforming Temperature on Structure and Precipitates of 0.05C-0.13Nb Steel
Effect of Hot Rolled Cooling Process on Structure and Properties of Nb-Ti Microalloy Dual Phase Steel
Effect of Solution Heat Treatment Temperature and Cooling Mode on Microstructure and Mechanical Property of Ni-Cr-Mo-Co Alloy
Mechanical Properties of Ni-Cr-Al Alloy Cold Drawn Bar
Effect of Cold Drawing Deformation and Annealing Treatment on Microstructure and Properties of GH4169 Wire

Related Author

文建华
孙新军
刘清友
阴树标
项金钟
陈连生
那顺桑
狄国标

Related Institution

云南大学物理科学技术学院
钢铁研究总院结构材料研究所
轧制技术及连轧自动化国家重点实验室(东北大学)
河北理工大学冶金与能源学院
唐山国丰钢铁有限公司
0