Effect of Multihole Nozzle on Flow Field and Temperature Field of Liquid in Mold for Casting Bearing Steel 280 mm x 325 mm Bloom
更新时间:2026-01-21
    • Effect of Multihole Nozzle on Flow Field and Temperature Field of Liquid in Mold for Casting Bearing Steel 280 mm x 325 mm Bloom

    • Special Steel   Vol. 37, Issue 2, Pages: 12-15(2016)
    • Received:02 November 2015,

      Online First:05 August 2022,

      Published:05 August 2016

    移动端阅览

  • 党爱国, 崔娟, 刘敬军, et al. Effect of Multihole Nozzle on Flow Field and Temperature Field of Liquid in Mold for Casting Bearing Steel 280 mm x 325 mm Bloom[J]. Special Steel, 2016, 37(2): 12-15. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Numerical Simulation of Flow Field in Mould for Slab Continuous Casting and Optimal Operation
Numerical Simulation of Heat Transfer and Solidification of Liquid at Action of Flow Field in Mold for Slab
Numerical Simulation of Effect of 420 mm x 1100 mm Slab Casting Mold Injecting Argon on Flow Field and Temperature Field of Liquid
Simulation and Analysis on Solidification Structure of GCr15 Bearing Steel 280 mm x 325 mm Casting Bloom based on Finite Element Method
Nu merical Simulation of Temperature Field of 304 Stainless Steel Rod and Wire Hot Continuous Rolling

Related Author

贾凌锋
乐可襄
许长军
汪琦
胡林
刘良元
孙健
李永超

Related Institution

安徽工业大学冶金与资源学院
鞍钢集团朝阳鞍凌钢铁有限公司
辽宁科技大学材料与冶金学院
江苏科技大学张家港校区冶金与材料工程学院,张家港
太原科技大学工程力学系
0