Microstructure and Mechanical Properties of K465 Superalloy Prepared by Cold Crucible Levitation Melting
更新时间:2026-10-22
    • Microstructure and Mechanical Properties of K465 Superalloy Prepared by Cold Crucible Levitation Melting

    • Special Steel   Pages: 1-5(2026)
    • DOI:10.20057/j.1003-8620.N260113    

      CLC: TF133
    • Received:26 July 2026,

      Revised:2026-08-28,

      Accepted:08 September 2026,

      Online First:21 September 2026,

    移动端阅览

  • Pan Tao,Zhang Huaxia,Ma Xiuping,et al.Microstructure and Mechanical Properties of K465 Superalloy Prepared by Cold Crucible Levitation Melting[J].Special Steel, DOI:.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Austenitizing Temperature on Microstructure and Properties of 2 200 MPa Grade Ultra-High Strength Steel
Effect of High Temperature Tempering on Microstructure and Mechanical Properties of High Nitrogen Martensitic Stainless Bearing Steel
Effect of Heat Treatment Temperature on Microstructure and Properties of Fe-27Mn-9Al-1C-0.25V Low-density Steel
Effect of Heat Treatment Temperature on Microstructure and Properties of 0Cr21Al6 Hot Rolled Sheet
Progress in Research and Applications of Additive Manufacturing of High-Strength Steels

Related Author

Zhou Lei
Wang Fei
Zhang Hao
Yang Teng
Shi Zhiyue
Wang Rui
Qin Jin
Kang Yan

Related Institution

Technical Center of Baowu Special Metallurgy Co., Ltd.
School of Materials Science and Engineering, North University of China
Shanxi Key Laboratory of Advanced Metal Material for Special Environments, North University of China
State Key Laboratory of Advanced Stainless Steel
Shanxi Taigang Stainless Steel Co.,Ltd.
0