[1] |
Ni Zhuowen, Zhu Hongchun, Li Huabing, Jiang Zhouhua, Sun Zhengxin, He Zhiyu.
Analysis of the Types and Distribution of Inclusions in H13 Die Steel Electroslag Ingots
[J]. Special Steel, 2024, 45(6): 48-52.
|
[2] |
Wang Li, Liu Chengbao, Li Haoqiu, Wang Yi, Sun Zonghui, Liu Chunwei, Yang Chaoyun, Fu Zhihao.
Effect of Rare Earth on Inclusions and Fatigue Properties of 20CrMnTi Gear Steel
[J]. Special Steel, 2024, 45(6): 117-124.
|
[3] |
Yang Wenbin, Liu Zhongqiu, Wang Fang, Huang Xuechi, Lang Yuping, Li Baokuan.
Effect of Melting Rate on Solidification Process of High Filled Ratio 06Cr18Ni11Ti Electroslag Remelting Ingot
[J]. Special Steel, 2024, 45(6): 28-36.
|
[4] |
Xie Kang, Mo Jinqiang, Zhang Wei, Wang Lijun.
The Effect and Control of Rare Earth Ce on Carbonitrides Precipitation in 441 Ferritic Stainless Steel
[J]. Special Steel, 2024, 45(6): 1-7.
|
[5] |
Zheng Anmin, Fan Xuanyu, Huang Zengxin, Mao Wangwang, Yu Yanchong, Zhang Jinling, Wang Shebin.
Effect of Rare Earth Ce on the Evolution of Inclusions in 20MnTiB Cold Heading Steel
[J]. Special Steel, 2024, 45(6): 37-47.
|
[6] |
Zhao Haoqian, Zhang Yuming, Ma Bo, Gong Yanjie, Meng Yaoqing.
Effect of LF Soft Bubbling Time on Inclusions in Tire Cord Steel LX82 A
[J]. Special Steel, 2024, 45(6): 53-56.
|
[7] |
Yang Jianhua, Ju Yinjun, Yang Jun.
The Evolution Analysis and Removal of Oxide Inclusion in Tire Cord Steel XLX72 A
[J]. Special Steel, 2024, 45(5): 66-71.
|
[8] |
Wang Yuping, Wu Jianbo.
Application and Optimization of Mould Flow Field in 1000 mm-2200 mm Wide Slab Caster
[J]. Special Steel, 2024, 45(5): 85-89.
|
[9] |
Liu Yong, Zhang Yunfei, Zhao YingLi, Zhao Nan, Zhao Zhengrong, Fan Mingqiang, Tian Zhiqiang.
Smelting Process Practice to Improve the Cleanliness and Polishling Proptice of Die Steel
[J]. Special Steel, 2024, 45(5): 47-52.
|
[10] |
Xu Peng, Kang Xu, Cao Zhenwei, Wang Qiang, Liu Chong, Nian Baoguo.
Effect of Adding Direct Reduced Iron to EAF on Steelmaking
[J]. Special Steel, 2024, 45(5): 53-58.
|
[11] |
Yuan lin, Hu Xiaoqiang, Liu Yang, Li Dianzhong, Xie Jing, Chen Wei.
Comparative Analysis of 3%Cr Roller Steel by Rare Earth Refining and Electroslag Remelting
[J]. Special Steel, 2024, 45(5): 1-7.
|
[12] |
Cao Yulong, Zhang Saikang, Wang Xiuxiu, Ma Chongsheng, Li Guangqiang.
Effect of Heating Temperature on Decomposition Transition Behavior of M2C Carbide in High-vanadium High-speed Steel
[J]. Special Steel, 2024, 45(4): 146-152.
|
[13] |
Yang Shulei, Wang Xiwei, Tian Qiang, Wang Tiantian, Yang Shufeng.
Distribution Characteristics of Inclusions in GH4742 Superalloy Ingot by Vacuum Arc Remelting
[J]. Special Steel, 2024, 45(4): 61-67.
|
[14] |
Zhao Zimin, Sun Xin, Hou Dong, Zhou Weiji, Yao Yudong, Sun Changliang.
Transformation of the Completely Enclosed Atmosphere in Ordinary Electroslag Furnace and Its Influence on Typical Steel Grades
[J]. Special Steel, 2024, 45(4): 99-103.
|
[15] |
Sun Zhonghao, Li Qiang, Zhang Mingliang, Ma Chengkuan, Xia Zhibin, Zhong Yunbo.
Effect of Magnetic-Controlled Electroslag Remelting on Solidification Microstructure and Mechanical Properties of M2 High-speed Steel
[J]. Special Steel, 2024, 45(4): 68-76.
|