Numerical Simulation on Temperature Field of Hot Rolled Q215 Steel Bar Cooling by Turbulent Flow Process
Jin Yanjuan1, Zhang Zhu1, Cui Xiaochao1, Liu Yong2 , Sun Hongxiao2
1 School of Applied Science, Taiyuan University of Science and Technology, Taiyuan 030024;
2 Taiyuan Tiansong Engineering and Technology, Taiyuan 030024
Jin Yanjuan, Zhang Zhu, Cui Xiaochao, Liu Yong, Sun Hongxiao. Numerical Simulation on Temperature Field of Hot Rolled Q215 Steel Bar Cooling by Turbulent Flow Process[J]. Special Steel, 2007, 28(4): 24-26.
1李曼云.钢的控制轧制和控制冷却技术手册.北京:冶金工业出版社,1990
2赵宪明,吴迪,闻雷.大規格钢筋余热处理过程有限元分析与计算.材料科学与工艺,2002,10(1) :86
3于 伟,陈银莉,蔡庆伍.余热处理20MnSi带肋钢筋力学性能的模拟研究.特殊钢,2002,23(3):13
4孔祥谦.有限元法在传热学中的应用.北京:科学出版社,1998
5 Morals R D Loqez A G,Olivares L M. Heat Transfer Analysis during Water Spray Cooling of Steel Rods. ISIJ International 1990, 30 ⑴:48