Research Progress in Microalloyed Case-Hardened Steels for Gear

Ma Li, Wang Maoqiu , Dong Han   

  1. National Engineering Research Center of Advanced Steel Technology, Central Iron and Steel Research Institute, Beijing 100081
  • Received:2008-02-28 Online:2008-08-01 Published:2022-12-23

微合金化渗碳齿轮钢的研究进展

马 莉 , 王毛球, 董  瀚   

  1. 钢铁研究总院先进钢铁材料技术国家工程研究中心,北京100081
  • 作者简介:马 莉(1984-),女,硕士,高性能渗碳齿轮钢的基本力学
  • 基金资助:
    国家863计划新材料技术领域研究课题资助(编号  2006AA03Z526)

Abstract:  It  is  available  to  fine  grain  size  of case-hardened  steel  for  gear, increase  cutting  properties  and  fatigue property  of steel  by  adding  microalloying  elements  such  as  Al,Nb,Ti,N  and  B, while  to  shorten  carburizing  time, simplify  procedures  and  decrease  production  cost  by  adding  Nb,Ti  etc.elements.The  grade, chemical  compositions, production process characteristics and research progress of microalloying cold forging steels for gear, case-hardening steels for gear carburizing at high temperature and high strength-toughness steels for gear are presented in this article.

Key words:  Microalloying, Case-Hardened ,  Steel ,  for ,  Gear, Cold ,  Forging, Carburizing ,  at ,  High ,  Temperature, High Strength-Toughness

摘要: 通过添加Al、Nb、Tj、N和B等微合金化元素可细化渗碳齿轮钢的晶粒,提高切削性能和钢的疲劳性能;同时通过添加Nb、Ti等元素,可缩短渗碳时间,精简工序,降低成本。介绍了微合金化冷锻齿轮钢,高温渗碳齿轮钢,高强韧性齿轮钢的钢种、化学成分、生产工艺特点和研究进展。