ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2009, Vol. 30 ›› Issue (4): 19-21.

Previous Articles     Next Articles

A Study on Spread of 304 Stainless Steel Flat Wires during Rolling Process

Liu Shifeng, Xu Ping, Wang Bojian   

  1. Metallurgical Engineering College, Xi'an University of Architecture and Technology, Xi'an 710055
  • Received:2009-01-07 Online:2009-08-01 Published:2022-12-20

304不锈钢扁钢丝轧制过程中的宽展研究

刘世锋, 徐萍, 王伯健   

  1. 西安建筑科技大学冶金工程学院,西安710055
  • 作者简介:刘世锋(1978-),男,硕士,讲师,不锈钢制品的制备工艺及设备开发研究。

Abstract: Rules of spread for 304 austenite stainless steel ①5. 5 mm coil non-tension rolling by a Φ160 mm two-high mill at ambient with 33. 1% ~68. 0% reduction has been studied. Results showed that the change of spread was influenced by metal flow uniformity during rolling: as reduction Δh/h0 was less than 58. 9%, with increasing reduction ratio, the spread increased obviously, the formula of spread W1 '= 5. 11 (Δh/h0) +4. 92 was obtained and as the reduction was larger than 58.9%, with increasing reduction ratio, the spread increased a little due to more homogeneous deformation.

摘要: 研究了室温下304奥氏体不锈钢Φ5.5 mm盘条通过Φ160 mm二辊轧机经33.1%~68.0%压下量单道次无张力轧制的宽展规律。结果表明,宽展的变化受轧制过程中金属流动均匀程度的影响:当压下率Δh/h0小于58.9%时,随变形量增加,宽展增加明显,拟合得到宽展计算公式W1=5.11(Δh/h0)+4.92,当压下率大于58.9%时,变形较均匀,随压下量增加,宽展增加很小。