Special Steel ›› 2015, Vol. 36 ›› Issue (2): 60-61.
Previous Articles Next Articles
Zhang Xiuli1 , Sun Yongqing2 , Liang Jianxiong2 , Yang Zhiyong2 , Liu Zhenbao2 , Li Wenhui2
Received:
Online:
Published:
张秀丽1,孙永庆2,梁剑雄2,杨志勇2,刘振宝2,李文辉2
作者简介:
Abstract: The test steel 0Cr16Ni5Mo is melted by a 6 t vacuum induction furnace + electro-slag remelting process, forged to Φ120-160 mm steel products, finishing forging at ≥ 900 ℃, and the samples for mechanical properties test are treated at 950 ℃ for 1 h, air cooling + tempered at 520 ℃ for 4 h air cooling. The quantity regression relationships between composition and mechanical properties of products of steel 0Cr16Ni5Mo are obtained by regression analysis on steel products of 47 heats that are(σs=-1043.3+5507.6[C]-1177.0[Si]+212.6[Ni]+1160.3[Mo];σb=-648.2+4136.7[C]-424.7[Si]+137.2[Ni]+1018.4[Mo];A=11.9-137.6[C]+25.1[Si]-4.9[Ni]-2.5[Cr]-29.9[Mo];Akv=-473.3-451.3[Si]+103.3[Ni]+321.3[Mo], its significance level is 0.1.
Key words: Steel 0Cr16Ni5Mo, Φ120-160 mm Bar Products, Chemical Composition, Mechanical Properties, Regression Analysis
摘要: 0Cr16Ni5Mo钢由6 t真空感应炉+电渣重熔工艺冶炼,并锻造成Φ120~160 mm钢材,终锻温度≥900℃,力学性能试样经950℃ 1 h空冷+520℃ 4 h回火处理。对该钢47炉次的棒材回归分析,得到了0Cr16Ni5Mo钢材成分与力学性能的定量回归关系式:σs=-1043.3+5507.6[C]-1177.0[Si]+212.6[Ni]+1160.3[Mo];σb=-648.2+4136.7[C]-424.7[Si]+137.2[Ni]+1018.4[Mo];A=11.9-137.6[C]+25.1[Si]-4.9[Ni]-2.5[Cr]-29.9[Mo];Akv=-473.3-451.3[Si]+103.3[Ni]+321.3[Mo],其显著性水平为0.1。
关键词: 0Cr16Ni5Mo钢, Φ120 ~ 160 mm棒材, 化学成分, 力学性能, 回归分析
Zhang Xiuli , Sun Yongqing , Liang Jianxiong , Yang Zhiyong , Liu Zhenbao , Li Wenhui. Regression Analysis on Chemical Composition and Mechanical Properties of Steel 0Cr16Ni5Mo Φ120-160 mm Bar[J]. Special Steel, 2015, 36(2): 60-61.
张秀丽, 孙永庆, 梁剑雄, 杨志勇, 刘振宝, 李文辉. 0C16Ni5Mo钢Φ120 ~ 160 mm棒材成分和力学性能的回归分析[J]. 特殊钢, 2015, 36(2): 60-61.