ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2022, Vol. 43 ›› Issue (5): 51-54.

Special Issue: 电炉炼钢

Previous Articles     Next Articles

Development of 45Mn2R Sulfur Free-Cutting Steel for Automobile Parts

Liang Na , Liu Yongchang , Wang Sheng   

  1. Shandong Iron and Steel Company Ltd. , Laiwu 271105
  • Received:2022-03-08 Online:2022-10-01 Published:2022-09-28

汽车零部件用45Mn2R硫系易切削钢的开发

梁娜,刘永昌,王升   

  1. 山东钢铁股份有限公司,莱芜 271105
  • 作者简介:梁 娜(1982-),女,硕士,高级工程师

Abstract: The 45Mn2R steel Φ40-50 mm rolled product is developed by ≥ 40% hot metal- 50 t EAF-LF-VD-180 mm x 220 mm cast billet-rolling flow sheet. The cleanliness and casting ability are improved by controlling EAF end [C] ≥ 0.10% ,[P] ≤ 0.015% , tapping temperature 1 620-1 660 °C , preliminay deoxidation using " recaburizing agent + (15%Ca-12%Al-45%Si) compound deoxidation reagent + (50%CaO-34%A12O3-4%MgO) synthetic slag" during tapping, S content in metal ≤ 0.010% before Ca treatment, feeding S wire after Ca treatment for 20 min, soft blowing for 20 min after VD etc process measure. Results show that produced 45Mn2R steel (/% : 0.43-0.46C, 0.22-0.27Si, 0.009-0.017P, 0.065-0.086S, 0.32-0.36Cr, 0.003-0.010Ti, 0.013-0.034AIs) has better comprehensive properties to meet user requirement.

Key words: 45Mn2R Sulfur Free-Cutting Steel, ≥ 40% Hot Metal-50 t EAF-LF-VD-CC Flowsheet, Sulphide Control, Cleanliness

摘要: 采用≥40%铁水-50 t EAF-LF-VD-180 mm ×220 mm铸坯-轧制流程开发了45Mn2R钢Φ40~50 mm轧材。通过控制EAF终点[C]≥0.10%,[P]≤0.015%,出钢温度1620~1660℃,出钢过程用“增碳剂+复合脱氧剂(15%Ca-12%Al-45%Si)+合成渣(50%CaO-34%Al2O3-4%MgO)”预脱氧,Ca处理前钢水S含量≤0.010%,Ca处理20 min后喂S线,VD后软吹25~30 min等工艺措施,提升钢的纯净度和可浇性。结果表明,生产的45Mn2R钢(/%:0.43~0.46C,0.22~0.27Si, 0.009~0.017P,0.065~0.086S,0.32~0.36Cr, 0.003~0.010Ti, 0.013~0.034Als)具有良好的综合性能,各项指标满足用户要求。

关键词: 45Mn2R硫系易切削钢, ≥ 40%铁水-50 t EAF-LF-VD-CC流程, 硫化物控制, 洁净度